Industrial Grade 2 Titanium Sheet 2mm 3mm
video
Industrial Grade 2 Titanium Sheet 2mm 3mm

Industrial Grade 2 Titanium Sheet 2mm 3mm

Item name:Industrial Grade 2 titanium sheet 2mm 3mm
Thickness: From0.5mm~50mm
Material: CP Titanium Grade 1,Grade 2, Grade3

Standard: ASTM B265, AMS 4911
Zaslať požiadavku
Popis

Brief Data of Industrial Grade 2 titanium sheet 2mm 3mm

 

Standard: ASTM B265, AMS 4911

Grade:Grade 1,Grade 2,Grade 3

Size:Thickness 0.5mm~50.0mm*Width<1500mm*Length<6000mm

Features: The excellent properties of Titanium Plates include high strength, low density, good mechanical properties, corrosion resistance, high stability and so on. So Titanium & Titanium Alloy Plates always be used in airplane engine components, rockets, missile and other aircraft components.

In addition to that, titanium and titanium alloy plates also can be used in industrial construction , sports equipment, tableware, outdoor supplies and so on. The good performances of titanium plates make it easy to be accept and are more and more familiar by public.

 

Material Data of Industrial Grade 2 titanium sheet 2mm 3mm

 

 

4.51g/cc

0.163 lb/in³

 

98

98

 

38 MPa

5510 ksi

 

380 MPa

55100 psi

 

430 MPa

62400 psi

 

340 MPa

49300 psi

 

28%

28%

 

65 J

47.9 ft-lb

V-notch

 

Rolling Processing of Industrial Grade 2 titanium sheet 2mm 3mm

 

(1)Hot Rolled Processing:

Hot rolling is carried out above the recrystallization temperature of titanium alloys and is suitable for the production of medium-thickness plates (such as those with a thickness of more than 5mm). Hot rolling can enable titanium alloy plates to obtain good internal structure and mechanical properties, and improve the plasticity and toughness of the plates.

(2)Cold Rolled Processing:

Cold rolling is a rolling process carried out at room temperature, and is mainly used for the production of thin plates (such as those with a thickness ranging from 0.3 to 5mm), which can achieve higher surface accuracy and dimensional accuracy. The surface of the cold-rolled titanium alloy sheet is smooth and the thickness is uniform, making it suitable for components with high requirements for the surface quality of the sheet.

(3)Comparison of Rolling Processes:

Hot rolling and cold rolling both have their own advantages and disadvantages.

Hot rolling has a high production efficiency, but its surface quality is relatively poor.

Cold-rolled surfaces have good quality, but the production cost is relatively high.

In actual production, the appropriate rolling process can be selected according to the product requirements.

 

Ten Properties of Industrial Grade 2 titanium sheet 2mm 3mm

 

  • Non-magnetic, Non-toxic

 

Products Showcase of Industrial Grade 2 titanium sheet 2mm 3mm

 

Industrial Grade 2 titanium sheet 2mm 3mm
Industrial Grade 2 titanium sheet 2mm 3mm supplier
Industrial Grade 2 titanium sheet 2mm 3mm manufacturer
Industrial Grade 2 titanium sheet 2mm 3mm for sale

 

 

Baoji Reliab Metal Material Co.,Ltd is a professional manufacturer and supplier of Titanium mill products and Nickel,Zirconium products. With high quality controlling system, our products meeting the international standard as ASTM, ASME, AMS, JIS, DIN, TOCT, our main products including bars/rods, plates/sheets, tubes, wires, forgings rings, anodes, fasteners and CNC machined parts.

For over 11 years, Baoji Reliab Metal Material has grown as one of the steady suppliers for aerospace-grade titanium and medical-grade titanium products field in China.

Industrial Grade 2 titanium sheet 2mm 3mm made in China

 

Populárne Tagy: industrial grade 2 titanium sheet 2mm 3mm, China industrial grade 2 titanium sheet 2mm 3mm manufacturers, suppliers, factory, ASTM F136 TI6AL4V Eli Titanium Listy, CP2 Titánsky doštička ASTM B265, cena čistého titánu za kg, cena TiO2, titánová fólia, titánový oceľ

Zaslať požiadavku